MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Thermal Ceramics Kaocrete D Dense Castable
Categories: Ceramic; Oxide

Material Notes: Kaocrete D is a low-cost castable for service up to 2500°F (1371°C). For casting applications where thermal shock and moderate impact resistance is important.

Features:

  • Recommended use limit up to 3000°F (1649°C)
  • Aggregate chemistry and grain sizing
  • High purity binder systems
  • Installed by cast, gun or plaster
  • Applications:

  • Around water-cooled boiler tubes
  • Boiler ash hoppers
  • Kiln cars
  • Piers
  • Car bottoms
  • Seal tanks in FCCU vessels
  • Burner blocks
  • Ladle metallurgy lance material
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 2.019 - 2.179 g/ccFired
     
    Mechanical PropertiesOriginal ValueComments
    Modulus of Rupture 1.00 - 1.40 ksiDried 18-24 hours at 220°F; ASTM C133
     0.400 - 0.800 ksi
    @Treatment Temp. 816 °C,
    Time 18000 sec
    ASTM C133
     1.00 - 1.50 ksi
    @Treatment Temp. 1320 °C,
    Time 18000 sec
    ASTM C133
    Compressive Strength 24.1 - 41.4 MPaFired 5 hours at 1500°F
     31.0 - 41.4 MPaFired 5 hours at 2500°F
     31.0 - 48.3 MPaDried for 18-24 hours at 220°F
     
    Thermal PropertiesOriginal ValueComments
    Thermal Conductivity 0.890 W/m-K
    @Temperature 260 °C
     0.950 W/m-K
    @Temperature 538 °C
     0.980 W/m-K
    @Temperature 816 °C
     0.990 W/m-K
    @Temperature 1093 °C
    Maximum Service Temperature, Air 2500 °F
    Shrinkage 0.10 - 0.40 %
    @Temperature 816 °C,
    Time 18000 sec
    ASTM C113
     0.40 - 1.0 %
    @Temperature 1370 °C,
    Time 18000 sec
    ASTM C113
     0.00 - 0.20 %
    @Treatment Temp. 104 °C
    Dried 18-24 hours; ASTM C113
     
    Processing PropertiesOriginal ValueComments
    Shelf Life 12.0 Month
     
    Component Elements PropertiesOriginal ValueComments
    Al2O3 45 %
    Alkalis 0.30 %
    CaO 9.8 %
    Fe2O3 2.3 %
    SiO2 40 %
    TiO2 2.1 %
     
    Descriptive Properties
    MgO Contenttraces

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Thermal Ceramics Kaocrete B Dense Castable
    Pyrotek MT-29L Microporous Ladle Lining Insulation
    301 Stainless Steel

    CTHERM032 / 2352

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.