MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Excel Industries PEEB Ethyl-p-ethoxybenzoate, p-Ethoxy ehtylbenzoate
Categories: Other Engineering Material

Material Notes: CSA No: 23676-09-7

PEEB finds application as an important component in the catalyst system for the production of Polypropylene. It is used as inside electron donor in conjunction with a solid particulate catalyst precursor Triethylaluminium as co catalyst and an outside electron donor. Primary purpose of PEEB in the catalyst system is to function as the selectivity control agent. PEEB from Excel is a high purity product with extremely low levels of impurities and moisture. It is produced in state of the art plant at Roha using extremely sophisticated reaction and distillation systems. It has been successfully used in sustained production of Polypropylene since its launch in early 2002 and is now available for potential users all over the world.

Information provided by Excel Industries Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.071 - 1.075 g/cc
@Temperature 25.0 °C
Molecular Weight 194.23 g/mol
 
Descriptive Properties
Content<0.1%Ethyl alcohol
 <0.1%p-Ethoxy benzoic Acid
 <0.1%p-Hydroxy ethylbenzoate
 <500 ppmMoisture
Physical stateClear, colorless to pale yellow liquid
Purity>99.5%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEXCEL014 / 183490

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.