MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Phillips 66 IGL-9 Enclosed Gear Lubricant ISO 680, AGMA Number 8EP
Categories: Fluid; Lubricant

Material Notes: Description: Conoco IGL-9 Enclosed Gear Lubricant is a superior-quality, black, heavy, extreme-pressure gear lubricant developed specifically for enclosed gear sets operating under severe service conditions. IGL-9 Enclosed Gear Lubricant is available in ISO 460, 680 and 1000 viscosity grades. Each grade is formulated with high-quality paraffinic mineral oils and selected additives to provide rust and corrosion inhibition, demulsibility, resistance to foaming, excellent oxidation inhibition and superior load-carrying ability.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.926 g/cc0.0335 lb/in³
Viscosity Measurement 100100Viscosity Index
Saybolt Viscosity at 100°F 3180 SUS3180 SUS
Saybolt Viscosity at 210°F 220 SUS220 SUS
Kinematic Viscosity at 40°C (104°F) 660 cSt660 cSt
Kinematic Viscosity at 100°C (212°F) 46 cSt46 cSt
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Load Wear Index 5555
Four Ball Extreme Pressure, Weld Load 315 kg695 lb (mass)
Four Ball Wear 0.380 mm0.0150 in
Falex Load Test 5.85e+6 g12900 lbPin & Vee EP
Timken Test 34000 g75.0 lb
 
Thermal PropertiesMetricEnglishComments
Pour Point -15.0 °C5.00 °F
Flash Point 249 °C480 °F
 
Descriptive Properties
ColorBlack
FZG Gear TestPass 12 Stages

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON144 / 75181

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.