MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Parson Adhesives PARTITE® 7302 Methacrylate Structural Adhesive
Categories: Polymer; Adhesive

Material Notes: PARTITE 7302 is a two-component, 100% reactive, toughened structural methacrylate adhesive specifically formulated for bonding wide variety of metals, thermoplastics, thermosets, and composite assemblies with little to no surface preparation.

FEATURE:

  • Convenient 1:1 mix ratio, Non-sagging and thixotropic formulation
  • Excellent impact, peel and shear resistance
  • Non-sagging, gaps filled up to 0.50 inches.
  • Room temperature cures with very short open time.
APPLICATIONS:
  • Ideal for bonding all types of PVC, Polycarbonate, Acrylic, Fiberglass, PBT, PPO, ABS, FRT, Polyurethane, Epoxy, Wood, RIM, Nylon, FRP, Polyesters, Gelcoats, Styrene, Stainless Steel, Galvanized Steel, etc.
  • Ideal for Automotive Components, Sporting goods, Appliances, Computer Assemblies, Electrical Components, Furniture, Marine assemblies, Plastic Fabrications, Sign & Display, etc.

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.55 lb/galAdhesive
 8.59 lb/galMixed
 8.71 lb/galActivator
Brookfield Viscosity 80000 - 100000 cPRVT, Adhesive
 80000 - 100000 cPRVT, Activator
 210000 - 250000 cPMixed, Cure
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65 - 70ASTM D2240
Elongation at Break 19 %
Shear Strength 1500 psiABS/PVC; ASTM D1002
 1650 psiFiberglass; ASTM D1002
 >= 3200 psiAl/Al; ASTM D1002
 3950 psiSteel/Steel; ASTM D1002
 4200 psiDIN 53283
Tensile Impact 19.0 ft-lb/in
Peel Strength 15.0 - 20.0 pli
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -40.0 °F
Flash Point 51.0 °CAdhesive
 51.0 °CActivator
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hourFull
Working Life 1.00 - 2.00 min
 
Descriptive Properties
ColorMilky-WhiteAdhesive
 Off-WhiteActivator
Gap Filling<0.5 inCured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Parson Adhesives PARTITE® 7420 Methacrylate Structural Adhesive

PPARSN091 / 186534

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.