MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Solvay Chemicals Ammonium Hydrogen Fluoride
Categories: Fluid

Material Notes: Ammonium hydrogenfluoride (NH4HF2) is used for aluminum anodization, metal surface treatment, manufacture of wood preservatives, glass processing, building protection, mineral oil/ natural gas drilling, cleaning of industrial plants, in breweries and in the electronic industry

Ammonium bifluoride: CAS-No.: 1341-49-7 / EC-No.: 215-676-4 / Index-No.: 009-009-00-4
Ammonium fluoride: CAS-No.: 12125-01-8 / EC-No.: 235-185-9 / Index-No.: 009-006-00-8

Uses: Cleaning agent, Metal treatment, Non-metal-surface treatment products, Oil & gas industry and Chemical intermediate

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Molecular Weight 57 g/mol57 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 125.6 - 128 °C258.1 - 262 °F
Decomposition Temperature 239.5 - 240 °C463.1 - 464 °FThermal decomposition
 
Descriptive Properties
Appearanceflakes, strong hygroscopic
Colorwhite
Composition<4%Ammonium fluoride
 >94%Ammonium bifluoride

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay Chemicals Hydrogen Fluoride (HF)
EMS-Grivory Grivory® G4V-5H black 9915 PA*-GF50

WSOLV009 / 147658

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.