System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Lotte Advanced Materials Infino® HP-1000P PC/ABS, Unreinforced
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Polycarbonate/ABS Alloy, Unreinforced
;
Polycarbonate (PC)
Material Notes:
High flow material that can be used in the exterior material of mobile phone, wheel cap, rice cooker, electric iron etc. as well as refrigerator door handle and panel
Information provided by Samsung Cheil Industries.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.14
g/cc
ASTM D792
Linear Mold Shrinkage, Flow
0.0050
-
0.0070
cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow
22
g/10 min
@Load 10.0 kg,
Temperature 250 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Rockwell R
114
ASTM D785
Tensile Strength at Break
63.7
MPa
50 mm/min; ASTM D638
Tensile Strength, Yield
580
kg(f)/cm²
50 mm/min; ASTM D638
Elongation at Break
106 %
50 mm/min; ASTM D638
Tensile Modulus
20000
kg(f)/cm²
50 mm/min; ASTM D638
Flexural Strength
74.5
MPa
2.8 mm/min; ASTM D790
Flexural Modulus
20000
kg(f)/cm²
2.8 mm/min; ASTM D790
Izod Impact, Notched
53.0
kg-cm/cm
@Thickness 6.35 mm
ASTM D256
62.0
kg-cm/cm
@Thickness 3.17 mm
ASTM D256
Thermal Properties
Original Value
Comments
Deflection Temperature at 0.46 MPa (66 psi)
136
°C
@Thickness 6.40 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
124
°C
@Thickness 6.40 mm
ASTM D648
Vicat Softening Point
138
°C
B/50; ISO R306
140
°C
B/120; ISO R306
Flammability, UL94
HB
@Thickness 1.50 - 3.00 mm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Lotte Advanced Materials Infino® HP-1000H PC/ABS, Unreinforced
Lotte Advanced Materials Infino® HP-1000XD PC/ABS
Lotte Advanced Materials Infino® HP-1000XA PC/ABS, Unreinforced
Lotte Advanced Materials Infino® HI-1001BN PC/ABS, Unreinforced
Lotte Advanced Materials Infino® HP-1000XB PC/ABS
PSAMSU784 / 146601
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.