MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Multibase Nylex™ 1230 Natural Polyamide + PP
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polypropylene (PP)

Material Notes:

Features:

  • Crack Resistance, Good
  • Dimensional Stability, Good
  • Impact Resistance, Good
  • Moisture Resistant
  • Processability, Good
  • Forms:

  • Pellets
  • Processing Methods:

  • Injection Molding
  • Uses:

  • Electrical Parts
  • Housing, Electrical
  • Safety Equipment
  • Information provided by Multibase

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Specific Gravity 0.960 g/ccASTM 792
    Water Absorption 0.65 %ASTM D570
    Linear Mold Shrinkage 0.0050 cm/cmASTM D955
    Melt Flow 0.95 g/10 min
    @Load 2.16 kg,
    Temperature 230 °C
    ASTM D1238
     
    Mechanical PropertiesOriginal ValueComments
    Tensile Strength, Ultimate 3050 psiASTM D638
    Elongation at Break 160 %ASTM D638
    Flexural Strength 3000 psiASTM D790
    Flexural Modulus 122000 psiTangent; ASTM D790
    Izod Impact, Notched NB73°F; ASTM D256
    Gardner Impact 26.67 ft-lbASTM D3029
     
    Thermal PropertiesOriginal ValueComments
    Deflection Temperature at 0.46 MPa (66 psi) 347 °FUnannealed; ASTM D648
    Deflection Temperature at 1.8 MPa (264 psi) 257 °FUnannealed; ASTM D648
     
    Processing PropertiesOriginal ValueComments
    Rear Barrel Temperature 401 °F
    Middle Barrel Temperature 406 °F
    Front Barrel Temperature 415 °F
    Nozzle Temperature 415 °F
    Mold Temperature 55.4 - 118 °F
    Injection Pressure 350 - 1200 psi
    Back Pressure 50.0 - 150 psi
     
    Descriptive Properties
    Injection RateModerate-Fast

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Multibase Multi-Pro® 2510 XG Polypropylene
    Multibase Multi-Pro® 1004 R Polypropylene
    Multibase Multi-Flam™ 0801 PP Polypropylene
    Multibase Multibatch® MP 50004 Anti-split
    Multibase Multibatch® ME 50003 Anti-blocking Masterbatch

    PMULTI119 / 54023

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.