MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Elkem (Bluestar Silicones) SILCOLAPSE® RG 22 Foam Control Emulsion
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: SILCOLAPSE® RG 22 is a 20% active silicone emulsion designed for controlling foam in a wide range of aqueous or alcoholic media.

Applications:

  • Easy dispersion within aqueous media
  • Homogenous and stable emulsion
  • High foam control efficiency in many applications
Industries where SILCOLAPSE® RG 22 may be used:
  • Pulp and Paper: various processing steps (cooking, washing, screening, bleaching)
  • Detergency: liquids and powder detergents, soaps
  • Chemicals: distillations, extractions, filtrations
  • Oil Industries: extractions, butadiene process, amine-sweetening units
  • Water Treatment: biological step

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/cc
Solids Content 28 %28 %
pH 8.08.0
Storage Temperature 2.00 - 30.0 °C35.6 - 86.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Appearancewhite liquid
Content20% Active
Emulsifier typenon-ionic
Recommended dosage1-500 ppm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBLUST029 / 191005

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.