MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BYK Garamite® 2578 Rheological Additive for High Solids and Baking Enamels
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: General Description: GARAMITE™ 2578 is a unique rheological additive developed for high solids and baking enamels. GARAMITE™ 2578 is also recommended for use in high solids and thin film solvent based and 100% solids systems. Compared to fumed silica, GARAMITE™ 2578 provides improved sag resistance, rheology control and stability, is more efficient and is easier to handle in manufacturing (less dusty, higher bulk density and not sensitive to shear). GARAMITE™ 2578 will typically provide higher sag resistance, thermal slump resistance and settling resistance than thixotropes such as fumed silica, organoclays, hydrogenated castors, and polyamide waxes. GARAMITE™ 2578 will provide these superior properties at equal or lower viscosities than your current thixotrope. Because the recovery properties obtained with GARAMITE™ 2578 are unique, it is recommended application properties such as sag resistance or spray trials are used instead of viscosity to evaluate the efficiency of GARAMITE™ 2578. GARAMITE™ 2578 use levels are system dependent. A loading ladder from equal loading to 20-40% less than your current thixotrope should be evaluated. Air release agents such as BYK®-A 555* and rheological enhancers such as BYK®-R 605* (typically added at 5-10% based on the weight of GARAMITE™ 1958) are beneficial in many systems and may be included in the overall optimization evaluation.

Benefits:

  • Dispersion Ease
  • Low Viscosity/High Performance
  • Improved Thermal Slump Resistance
  • Viscosity Stability
  • Shear Stable
  • Syneresis Prevention
  • Settling Prevention
  • Sag Prevention
  • Increased Efficiency

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 8.00 lb/ft³
Density 1.50 - 1.70 g/cc
 
Component Elements PropertiesOriginal ValueComments
H2O, Water 6.0 %
 
Descriptive Properties
Color/FormOff white fine powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BYK Laponite® D Magnesium Silicate
BYK Laponite® B Fluorosilicate
BYK Gelwhite® LS Rheology Modifier
BYK Gelwhite® L Bentonite
BYK Gelwhite® H Bentonite

PBYK051 / 185048

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.