MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil Exact™ 4151 Ethylene-based Plastomer Resin
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Product Description: Exact 4151 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 4151 is designed for both monolayer and multilayer coextrusion cast and blown film applications requiring low sealing temperatures, high oxygen transmission and high toughness. Typical applications include seal layers for lamination films used in meat, poultry and produce packaging.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Blown Film
  • Lamination Film

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.895 g/ccExxonMobil method
Melt Flow 2.2 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 610 psiASTM D882
Film Tensile Strength at Yield, TD 580 psiASTM D882
Film Elongation at Yield, MD 10 %ASTM D882
Film Elongation at Yield, TD 9.0 %ASTM D882
Puncture Energy 67.0 in-lbExxonMobil Method
Elmendorf Tear Strength MD 220 gASTM D1922
Elmendorf Tear Strength TD 340 gASTM D1922
Dart Drop Test 1200 gASTM D1709A
Film Tensile Strength at Break, MD 11000 psiASTM D882
Film Tensile Strength at Break, TD 10000 psiASTM D882
1% Secant Modulus, MD 8100 psiASTM D882
1% Secant Modulus, TD 8800 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 190 °FPeak Melting Point; ExxonMobil method
Crystallization Temperature <= 160 °CPeak; ExxonMobil Method
Vicat Softening Point 169 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 5.1 %ASTM D1003
Gloss 70 %45°; ASTM D2457
 
Descriptive Properties
Puncture Force16 lbfExxonMobil Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Exact™ 3040 Cast Ethylene-based Plastomer Resin
ExxonMobil Escorene™ AD 0428EM1 Ethylene Vinyl Acetate Copolymer (European Grade)
ExxonMobil Enable™ 35-05HH Metallocene Polyethylene Resin
ExxonMobil Enable™ 20-10CB Metallocene Polyethylene Resin
ExxonMobil Enable™ 20-05HE Metallocene Polyethylene Resin

PEX99127 / 175363

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.