MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Nouryon Release Agent NL-1 Mixture of waxes, paste in solvents
Categories: Other Engineering Material

Material Notes: Release Agent NL-1 is an external Release Agent to facilitate demolding.

CAS number: 64742-82-1; 8002-74-2

EINECS/ELINCS No.: 265-185-4; 232-315-6

Applications: External Release Agent for use in unsaturated polyester resins: Release Agents are special products, which are used in the UP industry to enable a demoulding of the cured UP part from the mould. Release Agent NL-1 is a waxy paste, which must be applied as a first thin coat on the mould. After application the wax layer should be polished thoroughly. It is not necessary to renew the NL-1 layer after each demoulding. The number of demouldings in which the same wax layer will serve before it has to be renewed, depends on the material of which the mould is made, the demoulding time and the method of cleaning the mould. If the mould is washed out with water, containing detergents, renewal of the wax layer is necessary after each washing.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.800 g/cc
Volatiles 71 - 73 %
@Temperature 105 °C,
Time 7200 sec
 
Descriptive Properties
AppearanceFirm, white to yellowish paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY869 / 286392

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.