MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

General Plastics LAST-A-FOAM® FR-3730 Polyurethane Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Product Description: LAST-A-FOAM® FR-3700 is a CFC-free, rigid, closed-cell, flame-retardant polyurethane foam available in densities ranging from 3 to 40 pounds per cubic foot. Tougher and less friable than our FR-6700 series, this aerospace-grade, BMS 8-133-qualified foam enables cutting of crisper edges, making it well-suited to machining complex shapes for composite cores. It exhibits a high strength-to-weight ratio due to its cellular structure and cross-linked resin. Because of its closed-cell structure, LAST-A-FOAM® FR-3700 has excellent resistance to water absorption and will not swell, crack, or split on exposure to water. LAST-A-FOAM® FR-3700 provides exceptional protection for hazardous cargo and payloads as an impact- and fire-insulation liner in transport or packaging containers. It also serves as human bone test media.

Features:

  • Stable
  • Inert
  • Resistant to most chemicals and solvents
  • Easily shaped with common woodworking tools
  • Performs well as wood replacement
  • Will not support fungal growth
Applications:
  • Models and design prototypes
  • Composite Core
  • Honeycomb edge close-out for aircraft interior sandwich panels used in overhead storage bins, passenger cabin class dividers, galleys and lavatories
  • Vacuum form dies and mold patterns

Information provided by General Plastics Manufacturing Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.481 g/cc0.0174 lb/in³ASTM D1622
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 53.853.83 lbs/ft3, cut foam surface; ASTM D2240
 71.671.640 lbs/ft3, cut foam surface
Tensile Strength 12.67 MPa1838 psiParallel to Rise; ASTM D1623
 13.15 MPa1907 psiPerpendicular to Rise; ASTM D1623
Flexural Strength 17.27 MPa2505 psiRise Parallel to Beam Thick.; ASTM D790 Method 1-A
 19.04 MPa2761 psiRise Parallel to Test Span; ASTM D790 Method 1-A
Flexural Modulus 0.57825 GPa83.868 ksiRise Parallel to Test Span; ASTM D790 Method 1-A
 0.58480 GPa84.818 ksiRise Parallel to Beam Thick.; ASTM D790 Method 1-A
Compressive Strength  7.522 MPa
@Temperature 121 °C
1091 psi
@Temperature 250 °F
Parallel to Rise; ASTM D1621
 7.757 MPa
@Temperature 121 °C
1125 psi
@Temperature 250 °F
Perpendicular to Rise; ASTM D1621
 11.62 MPa
@Temperature 93.3 °C
1686 psi
@Temperature 200 °F
Parallel to Rise; ASTM D1621
 12.05 MPa
@Temperature 93.3 °C
1748 psi
@Temperature 200 °F
Perpendicular to Rise; ASTM D1621
 20.37 MPa
@Temperature 23.9 °C
2954 psi
@Temperature 75.0 °F
Parallel to Rise; ASTM D1621
 20.4 MPa
@Temperature 23.9 °C
2960 psi
@Temperature 75.0 °F
Perpendicular to Rise; ASTM D1621
 27.18 MPa
@Temperature -53.9 °C
3942 psi
@Temperature -65.0 °F
Parallel to Rise; ASTM D1621
 29.0 MPa
@Temperature -53.9 °C
4200 psi
@Temperature -65.0 °F
Perpendicular to Rise; ASTM D1621
Compressive Modulus  0.25792 GPa
@Temperature 121 °C
37.408 ksi
@Temperature 250 °F
Parallel to Rise; ASTM D1621
 0.26820 GPa
@Temperature 121 °C
38.899 ksi
@Temperature 250 °F
Perpendicular to Rise; ASTM D1621
 0.35204 GPa
@Temperature 23.9 °C
51.059 ksi
@Temperature 75.0 °F
Perpendicular to Rise; ASTM D1621
 0.3521 GPa
@Temperature 93.3 °C
51.07 ksi
@Temperature 200 °F
Parallel to Rise; ASTM D1621
 0.35498 GPa
@Temperature 23.9 °C
51.486 ksi
@Temperature 75.0 °F
Parallel to Rise; ASTM D1621
 0.36248 GPa
@Temperature 93.3 °C
52.573 ksi
@Temperature 200 °F
Perpendicular to Rise; ASTM D1621
 0.38324 GPa
@Temperature -53.9 °C
55.584 ksi
@Temperature -65.0 °F
Parallel to Rise; ASTM D1621
 0.4038 GPa
@Temperature -53.9 °C
58.57 ksi
@Temperature -65.0 °F
Perpendicular to Rise; ASTM D1621
Poissons Ratio 0.300.30
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 1.05 - 1.4
@Frequency 1e+6 Hz
1.05 - 1.4
@Frequency 1e+6 Hz
3-20 lbs/ft3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 63.0 µm/m-°C
@Temperature -45.6 - 93.3 °C
35.0 µin/in-°F
@Temperature -50.0 - 200 °F
GP Method
Specific Heat Capacity 1.48 J/g-°C0.353 BTU/lb-°FASTM E1269
Thermal Conductivity 0.0669 W/m-K0.464 BTU-in/hr-ft²-°FASTM C518
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -196 °C-320 °F
Glass Transition Temp, Tg 132 °C270 °FASTM E1824
 
Descriptive Properties
Closed Cell Content95%3 lbs/ft3, ASTM D2856, Procedure B
 99%25 lbs/ft3, ASTM D2856, Procedure B
Heat of Combustion11706 BTU/lbASTM D240
Tumbling Friability (%)0.140 lbs/ft3, 20 mins at 60 rpm, ASTM C421
 23.63 lbs/ft3, 20 mins at 60 rpm, ASTM C421
Water Absorption0.006 lbs/ft²at 18 lbs/ft³, ASTM D2842
 0.02 lbs/ft²at 3 lbs/ft³, ASTM D2842

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
General Plastics LAST-A-FOAM® FR-3818 FST Polyurethane Foam
BCC Products MB 1300 Polyurethane Foam Modeling Board
General Plastics LAST-A-FOAM® FR-10106 Polyurethane Foam
BCC Products MB 1200 Polyurethane Foam Modeling Board
Covestro Baynat® 3002 Polyurethane Foam

PGENR014 / 186800

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.