Product Description: LD 165 series are LDPE grades, offering high strength combined with medium optical properties. Availability: Africa & Middle East and Europe Additive: - Antiblock: No
- Slip: No
- Thermal Stabilizer: Yes
Applications: - Agriculture Film
- Blend Partner
- Construction Film
- Foam
- Heavy Duty Bags
- High Performance Collation Shrink
- Pallet Shrink Film
- Profile Extrusion
Information provided by ExxonMobil |