MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECAFIL PEI 9085 natura l- 1,75 mm - Filament Polyetherimide
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes:
  • inherent flame retardant
  • high dimensional stability
  • high thermal and mechanical capacity
  • resistance against high energy radiation
Target Industries:
  • electronics
  • automotive industry
  • mechanical engineering
  • aircraft and aerospace interiors
  • aircraft and aerospace technology

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³
Moisture Absorption 0.390 %0.390 %DIN EN ISO 62
Melt Flow 8.9 g/10 min
@Load 6.60 kg,
Temperature 295 °C
8.9 g/10 min
@Load 14.6 lb,
Temperature 563 °F
DIN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 49.0 MPa7110 psi5mm/min, Orientation ZX; DIN EN ISO 527-2
 80.0 MPa11600 psi5mm/min, Orientation XY; DIN EN ISO 527-2
Elongation at Break 2.6 %2.6 %5mm/min, Orientation ZX; DIN EN ISO 527-2
 9.3 %9.3 %5mm/min, Orientation XY; DIN EN ISO 527-2
Modulus of Elasticity 2.45 GPa355 ksi5mm/min, Orientation ZX; DIN EN ISO 527-2
 2.60 GPa377 ksi5mm/min, Orientation XY; DIN EN ISO 527-2
Flexural Strength 91.0 MPa13200 psi2mm/min, Orientation XY; DIN EN ISO 178
 93.0 MPa13500 psi2mm/min, Orientation ZX; DIN EN ISO 178
Flexural Modulus 2.12 GPa307 ksi2mm/min, Orientation XY; DIN EN ISO 178
 2.50 GPa363 ksi2mm/min, Orientation ZX; DIN EN ISO 178
Flexural Strain at Break 4.1 %4.1 %2mm/min, Orientation ZX; DIN EN ISO 178
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °Flong term
 170 °C338 °Fshort term
Deflection Temperature at 1.8 MPa (264 psi) 153 °C307 °FISO-R 75 Method A
Glass Transition Temp, Tg 180 °C356 °FASTM D3418
Flammability, UL94 V-0V-0125x13x1,5mm; DIN IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Processing Temperature 150 - 170 °C302 - 338 °FBuild chamber temperature
 160 - 190 °C320 - 374 °FPrint bed temperature
Nozzle Temperature 360 - 390 °C680 - 734 °FDiameter: 0,4 mm
Melt Temperature <= 410 °C<= 770 °F
Drying Temperature 120 °C248 °F
Dry Time 8.00 hour8.00 hour
 
Descriptive Properties
Colorbeige opaque
Fan speed0
Flammability1.5 mm60 sec. Vertical Bunsen Burner test, FAR §25.853 (a) and Appendix F, Part I, para. (a)(1)(i)
 1.5 mm12 sec. Vertical Bunsen Burner test, FAR §25.853 (a) and Appendix F, Part I, para. (a)(1)(ii)
 1.5 mm15 sec. Horizontal Bunsen Burner test, FAR §25.853 (a) and Appendix F, Part I, para. (a)(1)(iv)
 1.5 mmHeat Release, as per FAR §25.853 (d) and Appendix F, Part IV
 1.5 mmSmoke density, as per FAR §25.853 (d) and Appendix F, Part V
 1.5 mmGas Toxicity, as per Boeing BSS 7239
Print speed20-30 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIO1270 / 319198

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.