Product Description: PA 6, 30% Glass-fiber reinforced, Heat Stabilized, Lubricated, Post Industrial Recycled Feed stock, Black Color Availability: North America Filler/Reinforcement: Glass Fiber, 30% Filler by Weight Additive: Heat Stabilizer; Lubricant Recycled Content: Yes Features: Heat Stabilized; Lubricated RoSH Compliance: RoSH Compliant Appearance: Black Information provided by Ravago Manufacturing Americas |