ADVANCENE™ EE-1801-AAB is a part of a Butene LLDPE series offering excellent drawdown and puncture resistance combined with high gloss and clarity. They are also frequently used as a blend partner with LDPE resins to improve film properties and processability. Several additive packages are available according to the required surface properties. Applications: • Agricultural Film. • Bag in Box. • Barrier Food Packaging. • Blown Film. • Bread Bags. • Food Packaging. • Form Fill and Seal Packaging. • Freezer Film. • Garment Film. • General Packaging. • Heavy Duty Bags. • Ice Bags. • Industrial Liners. • Industrial Packaging. • Lamination Film. • Liners. • Multilayer Packaging Film. • Packaging Films. • Produce Bags. • Refuse Bags. • Shoppers. • Stand Up Pouches. • Trash Bags. Processing Notes: The film properties have been measured on 30 µm (1.18 mil) thick alms (Blow-up ratio : 2.5). Information provided by ETHYDCO. |