MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lanxess Santoweb® W Rubber Reinforcing Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Function: Santoweb W, a treated cellulose fiber product, provides reinforcement, increases product stiffness and reduces cut growth rate for NBR and Silicone rubber compounds, white compounds based on other rubber types and PVC.

Application: Santoweb W can be used for low pressure PVC hoses, medium pressure NBR hoses, gaskets, diaphragms, and vinyl flooring. Santoweb W is regulated for use in articles in contact with food as specified under BgVV XXI, Category 4. Santoweb W is not regulated for use in FDA food contact applications.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.47 g/cc
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
Appearancelight grey to cream fibers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Versalis Europrene® N OZO 5033 NBR-PVC blend
Lubrizol Advanced Materials Pearlstick® 45-50/29 Linear Thermoplastic Polyurethane Elastomer
LG Chemical LS100S PVC
LG Chemical LS100 PVC
Lanxess Ultramoll® V HV Plastic Additive

PLANY9055 / 209446

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.