MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chase Plastics CP Pryme® PC100RUL-10M BT Clear Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: 10 Melt, Prime Polycarbonate, Mold Release, UL-94 HB Rated, Blue Tint Clear Pellets.

Information provided by Chase Plastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Water Absorption 0.15 %0.15 %ASTM D570
Moisture Absorption at Equilibrium  0.35 %
@Temperature 22.8 °C
0.35 %
@Temperature 73.0 °F
ASTM D570
 0.58 %
@Temperature 100 °C
0.58 %
@Temperature 212 °F
ASTM D570
Melt Flow 11 g/10 min
@Load 1.20 kg,
Temperature 300 °C
11 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7070ASTM D785
Hardness, Rockwell R 118118ASTM D785
Tensile Strength at Break 68.9 MPa10000 psiType I, 2.0 in/min.; ASTM D638
Tensile Strength, Yield 62.1 MPa9000 psiType I, 2.0 in/min.; ASTM D638
Elongation at Break 130 %130 %Type I, 2.0 in/min.; ASTM D638
Elongation at Yield 7.0 %7.0 %Type I, 2.0 in/min.; ASTM D638
Flexural Yield Strength 96.5 MPa14000 psi0.051 in/min. 1.97 inch span; ASTM D790
Flexural Modulus 2.34 GPa340 ksi0.051 in/min. 1.97 inch span; ASTM D790
Izod Impact, Notched 8.01 J/cm
@Temperature 22.8 °C
15.0 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Izod Impact, Unnotched 32.0 J/cm
@Temperature 22.8 °C
60.0 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Gardner Impact 169 J
@Temperature 22.8 °C
125 ft-lb
@Temperature 73.0 °F
ASTM D3029
Tensile Impact Strength 578 kJ/m²275 ft-lb/in²Type S.; ASTM D1822
Dart Drop, Total Energy 63.9 J
@Temperature 22.8 °C
47.1 ft-lb
@Temperature 73.0 °F
ASTM D3763
Taber Abrasion, mg/1000 Cycles 10101000 g, CS-17 Wheel.; ASTM D1044
 
Thermal PropertiesMetricEnglishComments
CTE, linear 68.4 µm/m-°C
@Temperature -40.0 - 95.0 °C
38.0 µin/in-°F
@Temperature -40.0 - 203 °F
ASTM E831
Specific Heat Capacity 1.26 J/g-°C0.300 BTU/lb-°FASTM C351
Thermal Conductivity 0.274 W/m-K1.90 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
@Thickness 6.40 mm
280 °F
@Thickness 0.252 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
@Thickness 6.40 mm
270 °F
@Thickness 0.252 in
Unannealed; ASTM D648
Vicat Softening Point 154 °C310 °FRate B (120°C/h), Loading 2 (50 N).; ASTM D1525
Flammability, UL94 HBHB
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5861.586ASTM D542
Haze 1.0 %
@Thickness 2.54 mm
1.0 %
@Thickness 0.100 in
ASTM D1003
UV Transmittance 88 %
@Thickness 2.54 mm
88 %
@Thickness 0.100 in
ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHA936 / 268587

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.