MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Phillips 66 Megaplex® XD3 NGLI Grade 1
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Megaplex XD3 is a high-performance, multipurpose, extreme pressure (EP) lithium complex grease developed to satisfy the severe lubrication requirements of construction and off-road equipment manufactured by Caterpillar, Komatsu Dresser, Case New Holland, John Deere and others. It is particularly recommended for use in off-highway trucks and heavy equipment, such as bulldozers, motor graders and wheel loaders, operating under heavy or shock loads. Megaplex XD3 is manufactured with high-quality, heavy base oils, a special polymer, and a lithium complex soap thickener. It is fortified with extreme-pressure and antiwear additives, 3% molybdenum disulfide (moly), a tackifier, and rust and oxidation inhibitors to provide excellent wear protection as well as excellent corrosion protection and resistance to water washout in equipment operating under wet conditions and/or high temperatures and subject to heavy or shock loading. Megaplex XD3 Grade No. 1 is NLGI GC-LB certified for use as a multipurpose automotive wheel bearing and chassis lubricant.

Applications:

  • Chassis parts and wheel bearings of construction, mining and other heavy mobile equipment
  • Universal joints, constant velocity joints, brake self-adjusting screws and clutch release bearings on off-highway trucks and other heavy equipment
  • Tractor-trailer fifth wheels
  • Heavily loaded plain and rolling-element bearings in industrial and mobile equipment where the manufacturer specifies a high-temperature, extreme-pressure grease with 3% moly
Features/Benefit:
  • High dropping point (>500°F)
  • High load-carrying capacity
  • Excellent wear protection
  • Contains 3% moly for extra protection against galling and wear under shock loads
  • Excellent resistance to water washout
  • Excellent resistance to separation
  • Protects against rust and oxidation
  • NLGI GC-LB certified (Grade No. 1)

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.88 lb/gal
Viscosity Measurement 94Index
Saybolt Viscosity at 100°F 2470 SUS
Saybolt Viscosity at 210°F 147 SUS
Kinematic Viscosity at 40°C (104°F) 460 cSt
Kinematic Viscosity at 100°C (212°F) 30 cSt
Oxidative Stability 100 hour
@Pressure 0.0345 MPa
Pressure Drop; ASTM D942
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 400 kgASTM D2596
Four Ball Wear 0.550 mmScar Diameter; ASTM D2266
Penetration 310 - 340
Timken Test 55.0 lbOK Load; ASTM D2509
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 177 °C
Minimum Service Temperature, Air -23.0 °C
Dropping Point >= 260 °C
 
Descriptive Properties
ColorGray-Black
Composition3%Molybdenum Disulfide
ThickenerLithium Complex

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sumitomo Bakelite Durez® 19900 Phenolic Resin
Phillips 66 Multiplex® Red NGLI Grade 2
Kuraray SEPTON® A4 Hot Melt Adhesive
Kuraray SEPTON® A3 Hot Melt Adhesive
Kuraray SEPTON® A2 Hot Melt Adhesive

WCON5120 / 198373

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.