This concentrate contains 1% slow blooming slip (Erucamide) to improve the slip characteristics of polyethylene film. Can be used with clear films. Description/Features: Market: Processing Method: Note: Because Erucamide is an unsaturated molecule, this concentrate can have a limited shelf life under certain conditions. It is recommended to verify properties after six months. Acceptable for FDA applications depending on end use. Information provided by PolyOne Corporation. |