Description: 20-3001 NC is a low viscosity, unfilled epoxy potting and encapsulating system which forms a bubble free glass like finish when cured. This is a 100% solids resin system that does not contain any solvents. Its convenient 1:1 mix ratio and lack of fillers make it an ideal material for meter mix and dispense equipment. 20-3001 NC has been formulated for ease in handling. Its low viscosity aids in filling voids and air pockets. In addition, there is no filler settling with this system. 20-3001 NC is the non-crystallizing version of the original 20-3001 product.Information provided by Epoxies, Etc |