MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Teknor Apex APEX® S94-A0907C2-80NT Polyvinyl Chloride
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Notes: APEX S94-A0907C2-80NT is a Polyvinyl Chloride NSF Extrusion Compound available in opaque granular form. It complies with NSF/ANSI STANDARD 61.

Availability: Asia Pacific

Features: Non- DEHP Plasticizer

Uses: Hose

Form: Granules

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8686ASTM D2240
Tensile Strength at Break 20.0 MPa2900 psi0.2 in/min; ASTM D638
Elongation at Break 300 %300 %ASTM D638
 
Processing PropertiesMetricEnglishComments
Processing Temperature 155 - 165 °C311 - 329 °FCompression Zone
 160 - 170 °C320 - 338 °FMixing Zone
Feed Temperature 145 °C293 °F
Nozzle Temperature 170 - 185 °C338 - 365 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Formosa Plastics Formolon® 690 PVC
Denka VINYKON R2001 PVC, R grade for hard extrusion
Denka VINYKON M557050 PVC, M grade for soft injection molding
Colorite Polymers Flexchem 4051-02 Vinyl Compound
Colorite Polymers 9077 Non-Phthalate 77 Series Vinyl Compound

PTEKNQ0363 / 236854

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.