MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Chemlon® N60AHY Nylon 6, Dry, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Heat Stabilized

Material Notes: Notes: N60AHY is a high viscosity, unfilled, heat stabilized grade of nylon 6. It is primary intended for extrusion applications such as pipe and profile.

Availability: Europe

Additive: Heat Stabilizer

Features: Heat Stabilizer; High Viscosity

Uses: Piping Profiles

Processing Method: Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Moisture Absorption at Equilibrium 2.9 %2.9 %50% RH; ISO 62
Linear Mold Shrinkage 0.012 - 0.020 cm/cm0.012 - 0.020 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 70.3 MPa10200 psiISO 527-2
Tensile Modulus 3.00 GPa435 ksiISO 527-2
Flexural Strength 80.0 MPa11600 psiISO 178
Flexural Modulus 2.60 GPa377 ksiISO 178
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched 1.09 J/cm²5.20 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Strength 14.2 kV/mm
@Thickness 3.00 mm
360 kV/in
@Thickness 0.118 in
IEC 60243-1
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 190 °C374 °FUnannealed; ISO 72-2/B
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FUnannealed; ISO 72-2/A
 
Processing PropertiesMetricEnglishComments
Zone 1 230 - 250 °C446 - 482 °F
Zone 3 240 - 260 °C464 - 500 °F
Zone 5 240 - 260 °C464 - 500 °F
Melt Temperature 240 - 270 °C464 - 518 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 hour2.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Arlon 31580R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on an HDPE Carrier
Petromont 2200 High Density Polyethylene Resin
Nylene® NX4301 Nylon 6, Extrusion Grade
Nylene® 607 Nylon 6, Extrusion Grade
Nurel Engineering Polymers Promyde® B40 L PA 6, Dry, Lubricated

PTEKNQ0615 / 237106

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.