MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Hapco Hapsil 2463 Thermoset
Categories: Polymer; Thermoset

Material Notes: Steralloy™ is a specialty polymer series from Hapco that has been specifically formulated for applications where biocompatibility is required. Prototyping, food processing equipment, medical devices, prosthetics, and filtration are just a few of the applications where Steralloy™ is used.

Information provided by Hapco, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/ccASTM D-4669
Viscosity 5700 - 7700 cP5700 - 7700 cPASTM D-4878
Linear Mold Shrinkage 0.00050 - 0.0020 cm/cm0.00050 - 0.0020 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080ASTM D-2240
Tensile Strength 51.7 MPa7500 psiASTM D-638
Elongation at Break 6.0 %6.0 %ASTM D-638
Modulus of Elasticity 2.55 GPa370 ksiASTM D-638
Flexural Strength 71.0 MPa10300 psiASTM D-790
Flexural Modulus 1.37 GPa198 ksiASTM D-790
Izod Impact, Notched 0.107 J/cm0.200 ft-lb/inASTM D-256
Izod Impact, Unnotched 0.507 J/cm0.950 ft-lb/inASTM D-256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °C208 °FASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °C199 °FASTM D-648
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 240 min
@Thickness 3.17 mm,
Temperature 50.0 °C
2.00 - 4.00 hour
@Thickness 0.125 in,
Temperature 122 °F
Demold
 360 - 720 min
@Thickness 3.17 mm,
Temperature 25.0 °C
6.00 - 12.0 hour
@Thickness 0.125 in,
Temperature 77.0 °F
Demold
Gel Time 20.0 min
@Load 0.100 kg
20.0 min
@Load 0.221 lb
ASTM D-2971
 
Descriptive Properties
Color (cured)Clear/Pinkish Hue
Mix Ratio100:25Volume
 100:25Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHAPCO163 / 317222

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.