MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Lubrizol LifeSciences Isoplast® 2530 ETPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Isoplast® 2530 is an engineering thermoplastic polyurethane resin for medical applications.

Features: USP Class VI

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Water Absorption 0.13 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0060 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 55ASTM D648
Hardness, Rockwell R 121ASTM D648
Tensile Strength at Break 69.0 MPaASTM D638
Tensile Strength, Yield 63.0 MPaASTM D638
Elongation at Break 160 %ASTM D638
Elongation at Yield 6.0 %ASTM D638
Tensile Modulus 1900 MPaASTM D638
Flexural Strength 90.0 MPaASTM D790
Flexural Modulus 2300 MPaASTM D790
Izod Impact, Notched 59.0 J/m
@Thickness 3.20 mm,
Temperature -40.0 °C
ASTM D256
 85.0 J/m
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
Dart Drop, Total Energy 75.0 J
@Temperature -29.0 °C
ASTM D3763
 80.0 J
@Temperature 23.0 °C
ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 81.0 °Cunannealed; ASTM D648
 93.0 °Cannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °Cunannealed; ASTM D648
 89.0 °Cannealed; ASTM D648
Vicat Softening Point 101 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Yellow Index 10 %ASTM D1925
Transmission, Visible 96 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 221 - 243 °C
Mold Temperature 66.0 - 82.0 °C
Drying Temperature 85.0 - 91.0 °C
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol LifeSciences Isoplast® 2510 ETPU
Lubrizol LifeSciences Isoplast® 2530 White ETPU
Lubrizol ISOPLAST™ 202EZ Engineering Thermoplastic Polyurethane Resin
Lubrizol ISOPLAST™ 302EZ Engineering Thermoplastic Polyurethane Resin
Lubrizol LifeSciences Isoplast® 2531 ETPU

PLUBR9020 / 203587

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.