MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® M76/IM7 Curing Epoxy Matrix/Unidirectional Tape
Categories: Polymer; Thermoset; Epoxy

Material Notes:

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 700 MPaM76/42%/G1087/C, 5HS M46J high modulus fiber 275 gsm; pr EN 2561 type B
 718 MPaM76/42%/G793/C, 5HS high strength fiber 280 gsm; pr EN 2561 type B
 1030 MPaM76/42%/G1094/C, 5HS intermediate modulus fiber 290 gsm; pr EN 2561 type B
 90.0 MPa
@Temperature -59.4 °C
90°
 317 MPa
@Temperature -59.4 °C
Onset, Edge Delamination
 696 MPa
@Temperature -59.4 °C
Ultimate, Edge Delamination
 2447 MPa
@Temperature 23.9 °C
 2558 MPa
@Temperature -59.4 °C
Elongation at Break 1.12 %
@Temperature -59.4 °C
90°
 1.55 %
@Temperature -59.4 °C
 1.55 %
@Temperature 23.9 °C
Tensile Modulus 60.0 GPaM76/42%/G793/C, 5HS high strength fiber 280 gsm; pr EN 2561 type B
 68.0 GPaM76/42%/G1094/C, 5HS intermediate modulus fiber 290 gsm; pr EN 2561 type B
 102 GPaM76/42%/G1087/C, 5HS M46J high modulus fiber 275 gsm; pr EN 2561 type B
 2.90 GPa
@Temperature 104 °C
Wet, IPS Properties (±45° tension)
 3.20 GPa
@Temperature 93.3 °C
Wet, IPS Properties (±45° tension)
 4.20 GPa
@Temperature 82.2 °C
Wet, IPS Properties (±45° tension)
 5.20 GPa
@Temperature 23.9 °C
IPS Properties (±45 tension)
 8.40 GPa
@Temperature -59.4 °C
90°
 154 GPa
@Temperature 23.9 °C
 156 GPa
@Temperature -59.4 °C
Flexural Strength 1007 MPa
@Temperature 82.2 °C
0°, Wet
 1317 MPa
@Temperature 82.2 °C
0°, Dry
 1627 MPa
@Temperature 23.9 °C
Flexural Modulus 131 GPa
@Temperature 82.2 °C
0°, Wet
 135 GPa
@Temperature 82.2 °C
0°, Dry
 144 GPa
@Temperature 23.9 °C
Compressive Strength 276 MPaAfter Impact (25/50/25 orientation), 1500 in-lb/in. impact level
 228 MPa
@Temperature 82.2 °C
Open Hole (25/50/25 orientation), wet
 327 MPa
@Temperature 23.9 °C
Open Hole (25/50/25 orientation)
 495 MPa
@Temperature 98.9 °C
M76/42%/G1094/C, 5HS intermediate modulus fiber 290 gsm; pr EN 2850 type A
 569 MPa
@Temperature 98.9 °C
M76/42%/G1089/C, Twill 2x2 intermediate modulus fiber 200 gsm; pr EN 2850 type A
 651 MPa
@Temperature 23.3 °C
M76/42%/G1089/C, Twill 2x2 intermediate modulus fiber 200 gsm; pr EN 2850 type A
 695 MPa
@Temperature 23.3 °C
M76/42%/G1094/C, 5HS intermediate modulus fiber 290 gsm; pr EN 2850 type A
 1282 MPa
@Temperature 82.2 °C
0°, Wet
 1462 MPa
@Temperature 82.2 °C
0°, Dry
 1579 MPa
@Temperature 23.9 °C
Compressive Modulus 64000 MPa
@Temperature 23.3 °C
M76/42%/G1089/C, Twill 2x2 intermediate modulus fiber 200 gsm; pr EN 2850 type A
 70000 MPa
@Temperature 98.9 °C
M76/42%/G1094/C, 5HS intermediate modulus fiber 290 gsm; pr EN 2850 type A
 71000 MPa
@Temperature 98.9 °C
M76/42%/G1089/C, Twill 2x2 intermediate modulus fiber 200 gsm; pr EN 2850 type A
 71000 MPa
@Temperature 23.3 °C
M76/42%/G1094/C, 5HS intermediate modulus fiber 290 gsm; pr EN 2850 type A
Shear Strength 28.0 MPa
@Temperature 98.9 °C
Interlaminar, M76/42%/G1087/C, 5HS M46J high modulus fiber 275 gsm
 40.0 MPa
@Temperature 98.9 °C
Interlaminar, M76/42%/G1094/C, 5HS intermediate modulus fiber 290 gsm
 49.0 MPa
@Temperature 98.9 °C
Interlaminar, M76/42%/G793/C, 5HS high strength fiber 280 gsm
 61.0 MPa
@Temperature 98.9 °C
Interlaminar, M76/42%/G1089/C, Twill 2x2 intermediate modulus fiber 200 gsm
 64.0 MPa
@Temperature 23.3 °C
Interlaminar, M76/42%/G1087/C, 5HS M46J high modulus fiber 275 gsm
 75.0 MPa
@Temperature 82.2 °C
Interlaminar, 0°, Wet
 77.0 MPa
@Temperature 23.3 °C
Interlaminar, M76/42%/G1094/C, 5HS intermediate modulus fiber 290 gsm
 79.0 MPa
@Temperature 23.3 °C
Interlaminar, M76/42%/G793/C, 5HS high strength fiber 280 gsm
 90.0 MPa
@Temperature 23.3 °C
Interlaminar, M76/42%/G1089/C, Twill 2x2 intermediate modulus fiber 200 gsm
 99.0 MPa
@Temperature 82.2 °C
Interlaminar, 0°, Dry
 121 MPa
@Temperature 23.9 °C
Interlaminar, 0°
Tensile Impact 1.90 ft-lb/inInterlaminar Fracture, (DCB)
 1.90 ft-lb/inInterlaminar Fracture, (ENF)
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature -18.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHEXCB9151 / 322307

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.