MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Evonik VESTOPLAST® 408 Amorphous Polyalphaolefin
Categories: Polymer; Thermoplastic; Polyalphaolefin

Material Notes: VESTOPLAST 408 is a amorphous polyalphaolefin and butene-rich. Generally used as hot melt adhesives with high thermal stability under load for textile bonding and structural bonding.

Key Words: APAO
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/cc
@Temperature 23.0 °C
Viscosity 6000 - 10000 cP
@Temperature 190 °C
melt, rotational viscometer; DIN 53 019
Molecular Weight 11600 g/molMn; GPC
 48000 g/molMw; GPC
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 94DIN 53 505
Tensile Strength at Break 6.80 MPaDIN EN ISO 527-3
Elongation at Break 80 %DIN EN ISO 527-3
Shear Modulus 0.0700 GPa
@Temperature 23.0 °C
DIN EN ISO 6721-2
Penetration 3.0 - 7.0
@Thickness 0.100 mm
needle 100/25/5; DIN 52 010
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 100 - 105 °Cunder load 5 °C/h, weight 450g; Degussa Method
Glass Transition Temp, Tg -27.0 °CDSC
Ring & Ball Softening Point 114 - 122 °CDIN 52 011
 
Descriptive Properties
Open Time (sec)65Degussa Method
Setting Time (sec)1Degussa Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik VESTOPLAST® 703 Amorphous Polyalphaolefin
Evonik VESTOPLAST® 206 + 6%, 206 B Amorphous Polyalphaolefin
Evonik VESTOPLAST® EP NC 702 Amorphous Polyalphaolefin
Evonik VESTOPLAST® 750 Amorphous Polyalphaolefin
Evonik VESTOPLAST® 708 Amorphous Polyalphaolefin

PHUMB413 / 81415

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.