Standard grade UNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, and others, and extruding the composite resins into plates, and laminating and heat-pressing the plates. UNILATE plates and boards are superior in heat resistance, withstand voltage, strength, and processability to the plates and boards of thermoplastic resins such as nylon, polyacetal, and others. The UNILATE plates and boards are greatly improved in water-absorbing property, electrical properties, and processability, compared to other thermosetting resin laminated sheets used in electric insulation applications. Information provided by Unitika Ltd. |