MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Wacker® AKF 3385 Fluorosilicone Fluid
Categories: Fluid; Polymer

Material Notes: Product description: In comparison with conventional dimethyl or methyl phenyl polysiloxances, Wacker® AKF 3385 exhibits enhanced lubricity, anti-blocking distinct solubility and defoaming properties.

Properties: Wacker® AKF 3385 features low specific solubility, low surface tension and good spreading properties. It therefore functions as antifoam agent for solvent based systems as well as being able to withstand extreme conditions in which to defoam in. The high mechanical resistance of Wacker® AKF 3385 makes it suitable as a special base material for greases and pastes, which in addition to a good lubricating action, have to resist dissolving out. It exhibits a good oxidation and heat resistance which makes it conducive to extreme conditions.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/ccWSTM 3019
pH 5.5 - 7.0WSTM 3008
Viscosity 1000 - 7000 cP
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 101.1 °CClosed Cup; WSTM 3081
 
Descriptive Properties
Active ingredients (%)100
Appearancecolorless, clear to slightly turbid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Elastosil® FLR 3900/60 A/B Liquid Fluorosilicone Rubber
Shin-Etsu Silicones FE-221U Fluorosilicone Elastomer
Saint-Gobain COHRlastic® R10490 Medium Fluorosilicone Sponge Rubber
Precision Polymer Engineering F50A Fluorosilicone Rubber
P & P Technology EC-Q(F) Fluorosilicone Elastomer

PWACK9728 / 205257

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.