MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Teijin Teijinconex® Middle Tenacity Meta-Aramid Fiber
Categories: Other Engineering Material; Composite Fibers; Polymer; Thermoset; Aramid

Material Notes: This polymetaphenylene isophthalic aramid organic lightweight synthetic fiber offers excellent resistance to heat, flame, and chemicals – enabling applications that are stronger, lighter and more durable. In particular, Teijinconex® is ideal for the manufacture of protective clothing and other industrial applications, including automotive hoses, industrial felt, filters, copy cleaners and much more.

Information provided by Teijin Aramid B.V.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³
Moisture Absorption 5.25 %5.25 %
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 39.5 %39.5 %
Tenacity 0.494 N/tex5.60 g/denier
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0400 - 0.0500 W/m-K0.278 - 0.347 BTU-in/hr-ft²-°Fmeasured in a fabric
Maximum Service Temperature, Air 230 °C446 °F100% strength retention at 100 hours
Decomposition Temperature >= 400 °C>= 752 °F
Oxygen Index 27 - 38 %27 - 38 %measured in a fabric

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEIH995b / 287680

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.