MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Thermal Ceramics Kaofil Moldable
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Kaofil Moldable is a mixture of ceramic fiber, silica binders, and fillers which produces an insulating product with a semi-sticky consistency. This type of mix is ideal for applications such as penetration seals, metal stud protection (as in ceramic cone anchors), and for patching refractory cracks and fissures. The temperature of Kaofil Moldable and any surface to which it is to be applied should be 70°F (20°C) or above to ensure proper adhesion.

Drying is possible at room temperature; but depending on thickness, may require an extended period of time. Heated, forced air drying is recommended. This may be safely accomplished at any internal temperature below 212°F (100°C). Ventilation should be provided during drying to exhaust organic fumes resulting from vaporization of certain organic agents.

Features:

  • High-temperature putty
  • Ready to use
  • Easy to apply
  • Air dries and hardens
  • Applications:

  • Metal stud protection
  • Patching mix for ceramic fiber and refractory products
  • Trough linings for aluminum and other non-ferrous metals
  • Patching around burner blocks
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.753 g/cc0.0272 lb/in³dry
     1.20 - 1.28 g/cc0.0434 - 0.0462 lb/in³wet
    Solids Content 51 %51 %
    pH 9.0 - 109.0 - 10
     
    Mechanical PropertiesMetricEnglishComments
    Modulus of Rupture 0.00172 GPa0.250 ksiDried
     
    Thermal PropertiesMetricEnglishComments
    Melting Point 1760 °C3200 °F
    Maximum Service Temperature, Air 1260 °C2300 °F
    Shrinkage  0.20 %
    @Temperature 104 °C,
    Time 86400 sec
    0.20 %
    @Temperature 220 °F,
    Time 24.0 hour
    drying
     3.0 %
    @Temperature 1090 °C,
    Time 18000 sec
    3.0 %
    @Temperature 2000 °F,
    Time 5.00 hour
     
    Processing PropertiesMetricEnglishComments
    Shelf Life 6.00 Month6.00 Month
     
    Component Elements PropertiesMetricEnglishComments
    Al2O3 30 %30 %
    SiO2 70 %70 %
     
    Descriptive Properties
    Hot gas erosion resistance, ft/sec>200

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    CTHERM266 / 2586

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.