MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SunChemical Gwent C2050517D1 Carbon Graphite Ink
Categories: Fluid; Metal; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: This is designed for screen-printing of working electrodes for electrochemical sensors. The paste is highly thixotropic which gives it very good definition on printing. This product has been designed to be compatible with Polymer Silver which can be printed underneath the carbon to improve the conductivity of the printed electrodes. Product Benefits: Low coefficient of variation (CV%), no significant hazardous Materials.
Screen Printing Equipment: semi-automatic, manual
Screen Types: stainless steel, polyester, mesh 156-230tpi
Substrate: polyester, PVC, polycarbonate or ceramic

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 40.59 - 44.41 %
@Temperature 130 °C
90 min
Viscosity 3400 - 4600 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
Haake VT 550 PK1.1°
Thickness 24.0 micronsCured, Printed through 230 stainless steel mesh with 13 micron emulsion
Storage Temperature 20.0 °Csealed container
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 107 ohmPrinted through 230 stainless steel mesh with 13 micron emulsion
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 min
@Temperature 130 °C
Shelf Life 6.00 Month
 
Descriptive Properties
Coverage cm2/g541Using a 230 mesh stainless steel screen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond LED401 White One Component LED Curable Adhesive System
California Fine Wire Nickel 211 (Nickel Manganese Alloy)
SunChemical Gwent C2020422D6 Nickel Electrode Ink

WGELZ9006 / 139319

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.