MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Solvay BR® 127 Corrosion Inhibiting Epoxy Primer
Categories: Polymer; Thermoset; Epoxy

Material Notes: BR® 127 corrosion inhibiting primer is a modified epoxy primer. It is a high-performance corrosion inhibiting primer and has been used in many commercial aircraft built since its introduction. BR 127 primer can be used with essentially all 250°F (121°C) film adhesives and has been designed to provide optimal structural performance at temperatures ranging from -67°F to 300°F (-55°C to 149°C). BR 127 primer is formulated to provide maximum environmental resistance and durability within the bond line, as well as prevent corrosive undercutting. It can also be used effectively as a protective coating outside bonded areas. BR 127 corrosion inhibiting primer can be cured prior to bonding. Recommended cure cycles range from 4 hours at 180°F (82°C) to 30 minutes at 250°F (121°C). Articles primed with BR 127 primer and then cured have an indefinite shelf life. Primed details should be wrapped in Kraft paper (as protection from dust and dirt) and stored prior to adhesive bonding. Maintaining controlled conditions of 85°F (29°C) maximum temperature and 65% maximum humidity is recommended for extended storage life. Cure cycles for adhesive films primed with BR 127 primer may vary from 200°F to 350°F (93°C to 177°C) with minimum pressures to assure proper mating of bonded details.

Features & Benefits:

  • Industry-wide standard for corrosion resistant primers
  • Prevents hydrolysis of oxide layers
  • Structural performance from -67°F to 300°F (-55°C to 149°C)
  • Compatible with a wide variety of adhesive systems
  • Improves hydrolytic stability at the adhesive-to-metal interface
  • Protects prepared surfaces from further oxidation

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.875 g/cc0.0316 lb/in³
Solids Content 9.0 - 11 %9.0 - 11 %sprayable
Volatile Organic Compounds (VOC) Content 792 g/l792 g/l
Outgassing - Total Mass Loss 0.48 %0.48 %
Collected Volatile Condensable Material 0.030 %0.030 %
Storage Temperature -18.0 °C-0.400 °F
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 39.2 MPa5680 psiLap, Initial
 30.9 MPa
@Time 1.56e+7 sec
4480 psi
@Time 4320 hour
Lap
 34.3 MPa
@Time 7.78e+6 sec
4970 psi
@Time 2160 hour
Lap
 40.6 MPa
@Time 2.59e+6 sec
5890 psi
@Time 720 hour
Lap
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °FStructural performance
Minimum Service Temperature, Air -55.0 °C-67.0 °FStructural performance
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorYellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Northern White Pine Wood
American Pine Wood
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
Overview of materials for Thermoset Polyurethane Foam, Glass Filled
3M ATG 987 Tape

PCYTED002p / 240083

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.