MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Solvay Chemicals SOLKANE® 410A
Categories: Fluid

Material Notes: HFC SOLKANE® 410A is a substitute for R22 and R13B1. It substitutes R22 in small air conditioning and transport refrigeration units as well as R13B1 for low temperature applications in temperature ranges from -70°C up to -40°C.

Pentafluoroethane- CAS-No.: 354-33-6 / EC-No.: 206-557-8 / REACH Registration Number: 01-2119485636-25 and Difluoromethane- CAS-No.: 75-10-5 / EC-No.: 200-839-4

Uses: Refrigerant

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Melting Point -103 °C-153 °FPentafluoroethane
Boiling Point -52.7 °C-62.9 °F
 
Descriptive Properties
Appearancecompressed liquefied gas
Colorcolorless
Composition0.5Pentafluoroethane
 0.5Difluoromethane

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Honeywell Genetron® 134a Refrigerant
Honeywell Genetron® 404A Refrigerant

WSOLV080 / 147729

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.