MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Petra® 130 FR 30% Glass Filled PET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant

Material Notes: Petra 130 FR is a 30% glass fiber reinforced, flame retardant injection molding polyethylene terephthalate feedstocks. It is recognized as UL 94V-0/5VA by Underwriters Laboratories. It is also available in pigmented versions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.68 g/ccISO 1183
Viscosity Measurement 0.49Inherent Viscosity
Linear Mold Shrinkage 0.0030 cm/cmASTM Data; MD
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118ASTM Test
Tensile Strength at Break 130 MPa0.2 in/min; ASTM Test
Tensile Strength, Ultimate 130 MPa5mm/min; ISO 527
Elongation at Break 2.0 %5mm/min; ISO 527
 2.0 %0.2 in/min; ASTM Test
Tensile Modulus 11100 MPa1mm/min; ISO 527
Flexural Strength 210 MPaASTM Test
 85.0 MPa
@Temperature 120 °C
ASTM Test
 275 MPa
@Temperature -40.0 °C
ASTM Test
Flexural Modulus 9700 MPaASTM Test
 2970 MPa
@Temperature 120 °C
ASTM Test
Izod Impact, Notched 0.900 J/cm
@Thickness 3.17 mm
ASTM Test
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 60093
Dielectric Constant 3.6
@Frequency 1e+6 Hz
IEC 60250
 3.8
@Frequency 100 Hz
IEC 60250
Dielectric Strength 40.0 kV/mmIEC 60243-1
Dissipation Factor 0.020
@Frequency 1e+6 Hz
IEC 60250
 0.020
@Frequency 100 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 24.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM Test
CTE, linear, Parallel to Flow 24.0 µm/m-°CASTM Test
Melting Point 245 °C10 K/min
 245 °CASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 240 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 210 °CISO 75
 220 °CASTM Test
Flammability, UL94 V-0
@Thickness 0.300 mm
 V-0
@Thickness 3.00 mm
 5VA
@Thickness 0.800 mm
Oxygen Index 36 %ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 275 °CInjection molding
Mold Temperature 115 °CInjection molding
Injection Velocity 115 mm/secInjection molding
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
FormPellets
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
Special characteristicFlame retarding agent
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Petra® 130 30% Glass Filled PET
BASF Petra® 130 FR BK-112 30% Glass Filled PET
BASF Petra® 330 FR BK-112 30% Glass Filled PET
BASF Petra® 130 BK-112 30% Glass Filled PET
Celanese Rynite® FR530 NC010 PET-GF30FR(17)

PBASF9018 / 84782

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.