MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® 954-2A Curing Cyanate Resin, S-2 Glass Fiber Reinforced 8 Harness Satin Fabric
Categories: Polymer; Thermoset; Epoxy

Material Notes:

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 627 MPa
@Temperature 23.0 °C
Elongation at Yield 2.8 %
@Temperature 23.0 °C
Tensile Modulus 28.3 GPa
@Temperature 23.0 °C
Flexural Yield Strength 848 MPa
@Temperature 23.0 °C
Flexural Modulus 28.3 GPa
@Temperature 23.0 °C
Compressive Yield Strength 317 MPa
@Temperature 163 °C
0°, Wet
 345 MPa
@Temperature 149 °C
0°, Wet
 365 MPa
@Temperature 204 °C
 379 MPa
@Temperature 191 °C
 427 MPa
@Temperature 177 °C
 434 MPa
@Temperature 163 °C
 586 MPa
@Temperature 23.0 °C
Compressive Modulus 29.0 GPa
@Temperature 191 °C
 29.6 GPa
@Temperature 163 °C
 29.6 GPa
@Temperature 204 °C
 29.6 GPa
@Temperature 23.0 °C
 31.0 GPa
@Temperature 177 °C
Shear Strength 35.2 MPa
@Temperature 163 °C
Short Beam, Wet
 37.2 MPa
@Temperature 204 °C
Short Beam
 37.2 MPa
@Temperature 149 °C
Short Beam, Wet
 41.4 MPa
@Temperature 177 °C
Short Beam
 43.4 MPa
@Temperature 191 °C
Short Beam
 52.4 MPa
@Temperature 163 °C
Short Beam
 75.2 MPa
@Temperature 23.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexPly® 954-3 Curing Cyanate Resin
Park Aerospace Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 7781 E-Glass Reinforced
CRG Industries Advantic™ 30 Syntactic Foam
CRG Industries Advantic™ 40 Syntactic Foam
Hexcel® HexPly® 954-3A Curing Cyanate Resin

PHEXC023 / 98493

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.