MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Lupranate® MM103 Isocyanate Modified MDI
Categories: Fluid

Material Notes: Description: Lupranate® MM103 is a liquid carbodiimide modified 4,4’-diphenylmethane diisocyanate. Lupranate MM103 serves as the isocyanate component in the production of microcellular urethane elastomers. This product also may be used in combination with high molecular weight polyether polyols for the preparation of high grade flexible, semi-flexible and integral skin foam. It is also used in the preparation of prepolymers for elastomer, sealant, adhesive and coating applications.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/cc
Viscosity 40 cP
Vapor Pressure <= 1.33e-8 bar
@Temperature 25.0 °C
 
Thermal PropertiesOriginal ValueComments
Boiling Point >= 190 °C
@Pressure 0.000667 MPa
Flash Point 199 °C
 
Descriptive Properties
ColorLight Yellow
CompositionHydrolyzable Chlorine<30.0%
 NCO content0.295

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Lupranate® MS/264 Isocyanate
BASF Lupranate® MP102 Isocyanate Modified MDI
BASF Lupranate® MS Isocyanate
BASF Lupranate® R2500 Isocyanate
BASF Lupranate® 277 Isocyanate

PBASG0698 / 132331

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.