Kao-Lok Anchors, Washers and Studs are a combination refractory and stainless steel designed to be used with Thermal Ceramics blanket wallpaper furnace linings. Kao-Lok Anchor Systems have been one of the preferred methods of installing ceramic fiber wallpaper lining systems for more than 30 years.Information provided by Morgan Advanced Materials |