Solprene 200 is a medium cis polybutadiene with excellent mixing and processing behavior. It is used as ingredient in tire compounds and in other applications where good performance at low temperatures, excellent abrasion resistance, low heat build-up and good dynamic fatigue resistance are needed. It is packed in bales wrapped in low melting point polyethylene film. Applications: Information provided by Dynasol |