MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

UBE UPIA® AT (U-Varnish-A) 1001 Polyimide Film
Categories: Polymer; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: Polyimide film obtained from "UPIA®" exhibits a high thermal decomposition temperature. Especially, "UPIA®-ST (U-Varnish-S)" has a thermal decomposition temperature above 550°C, so it does not soften, fluidize, or decompose under use temperatures and it is able to be used in high-temperature processes. In addition, the polyimide coating has excellent dimensional stability even at high temperatures.

Information provided by UBE Industries, LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content  17 - 19 %
@Temperature 350 °C,
Time 1800 sec
17 - 19 %
@Temperature 662 °F,
Time 0.500 hour
 17 - 19 %
@Temperature 350 °C,
Time 1800 sec
17 - 19 %
@Temperature 662 °F,
Time 0.500 hour
Viscosity  5000 - 6000 cP
@Temperature 30.0 °C
5000 - 6000 cP
@Temperature 86.0 °F
E-type Solution Viscosity in NMP
 5000 - 6000 cP
@Temperature 30.0 °C
5000 - 6000 cP
@Temperature 86.0 °F
E-type Solution Viscosity in NMP
Thickness 20.0 microns0.787 mil
 50.0 microns1.97 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 229 MPa33200 psiASTM D882
 238 MPa34500 psiASTM D882
Elongation at Break 92 %92 %ASTM D882
 99 %99 %ASTM D882
Tensile Modulus 3.70 GPa537 ksiASTM D882
 3.70 GPa537 ksiASTM D882
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmASTM D257
 >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmASTM D257
Surface Resistance >= 1.00e+16 ohm>= 1.00e+16 ohmASTM D257
 >= 1.00e+16 ohm>= 1.00e+16 ohmASTM D257
Dielectric Strength 7.70 kV/mm196 kV/inASTM D149
 10.3 kV/mm262 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear  29.0 µm/m-°C
@Temperature 50.0 - 200 °C
16.1 µin/in-°F
@Temperature 122 - 392 °F
Fine linear dilatometer
 33.0 µm/m-°C
@Temperature 50.0 - 200 °C
18.3 µin/in-°F
@Temperature 122 - 392 °F
Fine linear dilatometer
Glass Transition Temp, Tg 274 °C525 °FFilm property; Dynamic viscoelasticity
 278 °C532 °FFilm property; Dynamic viscoelasticity
Decomposition Temperature >= 550 °C>= 1020 °F
 
Descriptive Properties
5% Weight Reduction Temp. (°C)592TGA. Film property
 599TGA. Film property
Chemical Resistance Elongation Retention (%)100Ethanol. Thickness: 20µm. 30°C, 24h Dipping.
 102Trichloroethylene. Thickness: 20µm. 30°C, 24h Dipping.
 107N-methyl-2-pyroridon. Thickness: 20µm. 30°C, 24h Dipping.
 108Glacial acetic acid. Thickness: 20µm. 30°C, 24h Dipping.
 8110% sodium hydroxide. Thickness: 20µm. 30°C, 24h Dipping.
 8210% hydrochloric acid. Thickness: 20µm. 30°C, 24h Dipping.
 84Xylene. Thickness: 20µm. 30°C, 24h Dipping.
 89Methyl ethyl ketone. Thickness: 20µm. 30°C, 24h Dipping.
 90Chloroform. Thickness: 20µm. 30°C, 24h Dipping
 90m-Cresol. Thickness: 20µm. 30°C, 24h Dipping.
 912% sodium hydroxide. Thickness: 20µm. 30°C, 24h Dipping.
 9410% sulfuric acid. Thickness: 20µm. 30°C, 24h Dipping.
 96Methylene chloride. Thickness: 20µm. 30°C, 24h Dipping.
Chemical Resistance Strength Retention (%)8210% sodium hydroxide. Thickness: 20µm. 30°C, 24h Dipping.
 88Chloroform. Thickness: 20µm. 30°C, 24h Dipping
 89Ethanol. Thickness: 20µm. 30°C, 24h Dipping.
 90m-Cresol. Thickness: 20µm. 30°C, 24h Dipping.
 91Glacial acetic acid. Thickness: 20µm. 30°C, 24h Dipping.
 9110% hydrochloric acid. Thickness: 20µm. 30°C, 24h Dipping.
 92Methyl ethyl ketone. Thickness: 20µm. 30°C, 24h Dipping.
 9310% sulfuric acid. Thickness: 20µm. 30°C, 24h Dipping.
 93Trichloroethylene. Thickness: 20µm. 30°C, 24h Dipping.
 95Methylene chloride. Thickness: 20µm. 30°C, 24h Dipping.
 98N-methyl-2-pyroridon. Thickness: 20µm. 30°C, 24h Dipping.
 992% sodium hydroxide. Thickness: 20µm. 30°C, 24h Dipping.
 99Xylene. Thickness: 20µm. 30°C, 24h Dipping.
Heat Treatment Highest Temp.350
 350

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PUBD9858 / 287321

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.