MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Epoxies, Etc 20-1634 Lightweight Silicone Potting and Encapsulating Compound
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: 20-1634 is a low density, two component silicone elastomer. The 20-1634 is less than half the weight of most commercially available potting and encapsulating compounds. 20-1634 utilizes an advanced micro balloon technology filler. This system is ideal for applications that require low weight, flexibility, high heat resistance, and excellent electrical insulation properties. 20-1634 is formulated without solvents or other toxic materials. It is therefore not regulated or considered hazardous for transportation.

Features:

  • Low density
  • Flexible
  • Deep section curing (beyond 1-2 inches)
  • Solvent free
  • High operating temperatures
Benefits:
  • Does not add much weight to products
  • Low stress on components and vibration resistant
  • No need for multiple pours due to low exotherm
  • Good protection in extreme environmental applications
  • No by-products released during cure and safe to handle

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.800 g/ccResin (Part A)
 0.820 g/ccMixed
 0.970 g/ccActivator (Part B)
Viscosity 100 cPActivator (Part B)
 30000 cPMixed
 45000 cPResin (Part A)
Storage Temperature 18.0 - 27.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 34
Tensile Strength 125 psi
Elongation at Break 225 %
Tear Strength 16.5 pli
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cm
Dielectric Constant 3.1
@Frequency 100 Hz
Dielectric Strength 450 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 200 µm/m-°C
Thermal Conductivity 1.10 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 235 °C
Minimum Service Temperature, Air -65.0 °C
 
Processing PropertiesOriginal ValueComments
Pot Life 60.0 min
@Load 0.100 kg
Shelf Life 6.00 Month
 
Descriptive Properties
ColorClearActivator (Part B)
 WhiteResin (Part A)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PFEPOX002 / 316679

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.