MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chosun Refractories CTL-Z1 Monolithic Refractories for Ladle and Tundish
Categories: Ceramic

Material Notes:

Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 200 kg(f)/cm²
@Treatment Temp. 110 °C,
Time 86400 sec
Cold Crushing Strength
 350 kg(f)/cm²
@Treatment Temp. 1500 °C,
Time 10800 sec
Cold Crushing Strength
 
Thermal PropertiesOriginal ValueComments
Shrinkage 0.00 %
@Temperature 110 °C,
Time 86400 sec
 3.25 %
@Temperature 1500 °C,
Time 10800 sec
 
Component Elements PropertiesOriginal ValueComments
ZrO2 47 %
 
Descriptive Properties
Installation MethodCasting
Main ApplicationsWall
Material Required for Estimating (kg/m3)3,250
Water Required for Casting(%)6.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Garlock 2103 C.I. SBR/NBR Sheet Rubber, Polyester Insert
Industeel URANUS® S1 4 % Si, Austenitic Stainless Steel Resistant to Nitric Acid Solutions
Garlock 5260 Neoprene Sheet Rubber
EMS-Grivory Grilamid® 2D 25 W 20 HL X black 9992 PA612-I

CCHOS307 / 124251

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.