MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Lord Adhesives CoolTherm™ MD-161 Conductive Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: LORD CoolTherm™ MD-161 conductive adhesive offers excellent electrical conductivity. It is designed for dispensing through small nozzles. CoolTherm MD-161 adhesive provides excellent adhesion to a wide variety of surfaces including silicon, silver, gold and copper. Its excellent adhesion to SiC and GaN semiconductors make CoolTherm MD-161 adhesive ideally suited for demanding LED assembly applications.

Features: allows high-speed, accurate syringe dispensing of fine dots or lines; can be used with time/pressure, positive displacement or linear dispense heads; works with pin transfer equipment to precisely apply very fine dots. rapidly cures at 150°C. provides a working life of up to 5 days after loading a syringe into the dispensing equipment at room temperature.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 3.50 g/cc3.50 g/cc
Viscosity 40000 cP
@Temperature 25.0 °C
40000 cP
@Temperature 77.0 °F
40 mm, Cone 1, 2 sec^-1
 
Mechanical PropertiesMetricEnglishComments
Shear Strength  2.76 MPa
@Temperature 300 °C
400 psi
@Temperature 572 °F
Die Shear, cured, 80x80mil Silicon Die to Nickel Plated Copper
 4.83 MPa
@Temperature 250 °C
700 psi
@Temperature 482 °F
Die Shear, cured, 80x80mil Silicon Die to Nickel Plated Copper
 6.21 MPa
@Temperature 200 °C
900 psi
@Temperature 392 °F
Die Shear, cured, 80x80mil Silicon Die to Nickel Plated Copper
 16.5 MPa
@Temperature 150 °C
2400 psi
@Temperature 302 °F
Die Shear, cured, 80x80mil Silicon Die to Nickel Plated Copper
 44.8 MPa
@Temperature 25.0 °C
6500 psi
@Temperature 77.0 °F
Die Shear, cured, 80x80mil Silicon Die to Nickel Plated Copper
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.0 µm/m-°C27.8 µin/in-°Falpha 1 cured
 180 µm/m-°C100 µin/in-°Falpha 2, cured
Thermal Conductivity 1.90 W/m-K13.2 BTU-in/hr-ft²-°Fcured
Glass Transition Temp, Tg 55.0 °C131 °Fby TMA, cured
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month
@Temperature -30.0 °C
6.00 Month
@Temperature -22.0 °F
from date of manufacture when stored in original, unopened container
 
Descriptive Properties
AppearanceSilver Paste
Storage Modulus5000 MPa25C, cured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLORD9234 / 232590

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.