MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Iran Petrochemical (PCC) I1 HA 7260 High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: I1 (HA 7260) is a high density polyethylene with propylene as comonomer. It is very easy flowing, high density, hardness and stiffness, largely warpage free, for mass product articles in rapid shot frequence.

Applications: lightweight household, disposable articles, large molding and complicated parts where high impact strength and stress cracking resistance is not demanded.

Information provided by Iran Petrochemical Commercial Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.957 g/ccISO 1183
Melt Flow 17 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 52 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Charpy Impact, Notched 2.00 kJ/m²ISO 179
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 280 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) EX 2 S HF 7750 M2 High Density Polyethylene
Iran Petrochemical (PCC) I4 HD 7255 High Density Polyethylene
Iran Petrochemical (PCC) I3S HC 7260(THE) High Density Polyethylene
Iran Petrochemical (PCC) BL2 HF 4750 High Density Polyethylene
Iran Petrochemical (PCC) EX 2 HF 7750 High Density Polyethylene

PIPC217 / 149679

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.