MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Master Bond X21Med One component primer/adhesive for polyolefins
Categories: Polymer; Adhesive

Material Notes: Key Features:
  • One component, easy to apply
  • Can be used as a primer or adhesive
  • Cures tough, not rigid
  • Cures at ambient or elevated temperatures
Master Bond X21Med is a specially formulated one component system for bonding and priming polyolefinic surfaces. X21Med is a very low viscosity (<250 cps) solvent based system that is easy to apply and process. Most often, it is used as a primer to promote adhesion of polyolefinic substrates to other kinds of materials, such as metals, ceramics, composites and other kinds of plastics. When employed as a primer, X21Med is applied in a very thin layer on to the polyolefinic piece and the solvent allowed to evaporate. This will take place typically in 2-4 hours and can be greatly accelerated by adding heat (15-30 minutes at 150-200°F). After the surface is primed in this manner, an epoxy or silicone is prepared and applied to the substrates, and then allowed to cure. When used in this fashion, X21Med is a bonding promoter, allowing adhesion to this low energy type of plastic (polyolefin) in a process that is relatively simple and straightforward. X21Med can also be used as an adhesive for bonding one polyolefin to another one. When used in this manner, a thin layer of X21Med is applied to each surface. The surfaces are then mated and the solvent is allowed to evaporate. When cured at room temperature, it will generally set up in 30-45 minutes with full cures in 12-24 hours. If cured at 150°F the curing time will be 1-2 hours. When being used as an adhesive, the maximum area of effectiveness for X21Med is about 1 square inch. When used as a primer, there is no such limitation in the size of the pieces. The polyolefin family of plastics is used in almost every kind of industry including aerospace, electronic, OEM, medical devices, among so many others. Using X21Med as a primer offers many advantages in handling and processing when compared to other methods of treating polyolefinic materials to allow for good adhesion.

Product Advantages:

  • Low viscosity, easy to apply
  • Can be used as an adhesive, primer or adhesion promoter
  • Surfaces primed with X21 are compatible with a wide variety of adhesives
  • Easier to use than other methods of pretreating polyolefinsl devices
  • Passes ISO 10993-5 for medical devices

Information provided by Masterbond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/cc
Solids Content 15 - 35 %15 - 35 %
Viscosity 30 - 250 cP30 - 250 cP
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.3 °C200 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
Glass Transition Temp, Tg 25.0 - 30.0 °C77.0 - 86.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 120 min
@Temperature 65.6 °C
1.00 - 2.00 hour
@Temperature 150 °F
 720 - 1440 min
@Temperature 23.9 °C
12.0 - 24.0 hour
@Temperature 75.0 °F
Shelf Life 6.00 Month6.00 MonthIn original unopened containers
 
Descriptive Properties
Colorclear to light amber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMASTM742 / 233799

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.