MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LEXAN™ Copolymer CFR5630 Polycarbonate (PC) (Asia)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LEXAN? CFR5630 Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density and 60 second vertical burn and OEM toxicity requirements. LEXAN CFR5630 resin is available in transparent and opaque colors.

Features: Low Smoke and Toxicity

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.110 %0.110 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.14 %0.14 %ISO 62-1
Viscosity 5.0 cP
@Load 1.20 kg,
Temperature 300 °C
5.0 cP
@Load 2.65 lb,
Temperature 572 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0055 - 0.0075 cm/cm
@Thickness 3.20 mm
0.0055 - 0.0075 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0060 - 0.0080 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 5.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
5.0 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 52.0 MPa7540 psi50 mm/min; ASTM D638
 52.0 MPa7540 psi50 mm/min; ISO 527
Tensile Strength, Yield 67.0 MPa9720 psi50 mm/min; ISO 527
 68.0 MPa9860 psi50 mm/min; ASTM D638
Elongation at Break 23 %23 %50 mm/min; ISO 527
 51 %51 %50 mm/min; ASTM D638
Elongation at Yield 6.0 %6.0 %50 mm/min; ASTM D638
 6.0 %6.0 %50 mm/min; ISO 527
Tensile Modulus 2.40 GPa348 ksi1 mm/min; ISO 527
 2.50 GPa363 ksi50 mm/min; ASTM D638
Flexural Strength 103 MPa14900 psiyield, 2 mm/min; ISO 178
 106 MPa15400 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.40 GPa348 ksi1.3 mm/min, 50 mm span; ASTM D790
 2.50 GPa363 ksi2 mm/min; ISO 178
Izod Impact Notched 100 J73.8 ft-lbASTM D256
 85.0 J
@Temperature -30.0 °C
62.7 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched 21.5 J/cm40.3 ft-lb/inASTM D4812
 20.0 J/cm
@Temperature -30.0 °C
37.5 ft-lb/in
@Temperature -22.0 °F
ASTM D4812
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²80*10*3; ISO 180/1A
 9.00 kJ/m²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NBNB80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
80*10*3; ISO 180/1U
Charpy Impact Unnotched 13.2 J/cm²62.8 ft-lb/in²Edgew 80*10*3 sp=62mm; ISO 179/1eU
 12.9 J/cm²
@Temperature -30.0 °C
61.4 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 0.900 J/cm²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 66.0 J48.7 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.79
@Frequency 1.10e+9 Hz
2.79
@Frequency 1.10e+9 Hz
ASTM ES 7-83
Dissipation Factor 0.0058
@Frequency 1.10e+9 Hz
0.0058
@Frequency 1.10e+9 Hz
ASTM ES 7-83
Comparative Tracking Index 175 - 250 V175 - 250 VUL 746A
Hot Wire Ignition, HWI  15 - 30 sec
@Thickness >=1.00 mm
15 - 30 sec
@Thickness >=0.0394 in
UL 746A
 30 - 60 sec
@Thickness >=3.00 mm
30 - 60 sec
@Thickness >=0.118 in
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness >=1.00 mm
>= 120 arcs
@Thickness >=0.0394 in
UL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  66.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
36.7 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 72.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
40.0 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow  70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 76.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
42.2 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
Hot Ball Pressure Test 125 °C257 °FPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 131 °C268 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
 131 °C
@Thickness 3.20 mm
268 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 120 °C248 °FEdgew 120*10*4 sp=100mm; ISO 75/Ae
 120 °C
@Thickness 3.20 mm
248 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 136 °C277 °FRate B/50; ASTM D1525
 137 °C279 °FRate B/50; ISO 306
 139 °C282 °FRate B/120; ISO 306
UL RTI, Electrical 125 °C257 °FUL 746B
UL RTI, Mechanical with Impact 120 °C248 °FUL 746B
UL RTI, Mechanical without Impact 125 °C257 °FUL 746B
Flammability, UL94  V-2
@Thickness >=0.400 mm
V-2
@Thickness >=0.0157 in
UL 94
 V-0
@Thickness >=1.00 mm
V-0
@Thickness >=0.0394 in
UL 94
 5VA
@Thickness >=3.00 mm
5VA
@Thickness >=0.118 in
UL 94
Smoke Density <= 100<= 100Flaming, Dmax; ASTM E662
Oxygen Index 45 %45 %ISO 4589
Glow Wire Ignition Temperature  850 °C
@Thickness 3.00 mm
1560 °F
@Thickness 0.118 in
IEC 60695-2-13
 875 °C
@Thickness 1.00 mm
1610 °F
@Thickness 0.0394 in
IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 280 - 305 °C536 - 581 °F
Zone 2 275 - 300 °C527 - 572 °F
Zone 3 290 - 310 °C554 - 590 °F
Melt Temperature 290 - 310 °C554 - 590 °FInjection Molding
Mold Temperature 70.0 - 95.0 °C158 - 203 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 48.0 hour48.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm
 
Descriptive Properties
FAA Flammability, FAR 25.853 A/BPASSESFAR 25.853
UV-light, water exposure/immersionF1UL 746C
Vertical Burn a (60s) passes at5 SecondsFAR 25.853
Vertical Burn b (12s) passes at5 SecondsFAR 25.853

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80086 / 288033

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.