MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Akro-Plastic Akrotek® PK-VM CF 10 TM black (6135) Polyketone with Carbon Fiber
Categories: Polymer; Thermoplastic; Polyketone; Polyketone with Carbon Fiber

Material Notes: Carbon Fiber Reinforced Compounds. Very high elongation and excellent tribological performance. PK CF 10.

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³ISO 1183
Filler Content 10 %10 %ISO 1172
Linear Mold Shrinkage, Flow 0.014 - 0.016 cm/cm0.014 - 0.016 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.015 - 0.017 cm/cm0.015 - 0.017 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 59.0 MPa8560 psi5 mm/min. Conditioned; ISO 527-2
 59.0 MPa8560 psi5 mm/min. Dry as Molded; ISO 527-2
Elongation at Break >= 30 %>= 30 %5 mm/min. Conditioned; ISO 527-2
 >= 30 %>= 30 %5 mm/min. Dry as Molded; ISO 527-2
Tensile Modulus 3.40 GPa493 ksi1 mm/min. Conditioned; ISO 527-2
 3.50 GPa508 ksi1 mm/min. Dry as Molded.; ISO 527-2
Charpy Impact Unnotched  10.0 J/cm²
@Temperature 23.0 °C
47.6 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179-1/1eA
 10.0 J/cm²
@Temperature 23.0 °C
47.6 ft-lb/in²
@Temperature 73.4 °F
Dry as Molded; ISO 179-1/1eA
Charpy Impact, Notched 0.600 J/cm²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
Dry as Molded; ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+12 ohm1.00e+12 ohmDry as Molded; IEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FDry as Molded. DES, 10°C/min; DIN EN 11357-1
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Conditioned
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Dry as Molded
 
Descriptive Properties
Burning Rate<100 mm/minDry as Molded. FMVSS 302. >1 mm thickness
 <100 mm/minConditioned. FMVSS 302. >1 mm thickness

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKRO9886 / 255543

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.