MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
3M Scotch-Grip™ 826 Plastic Adhesive  (discontinued **)
Categories: Polymer; Adhesive; Thermoset

Material Notes: A high strength fast-drying adhesive with unique plastic bonding capabilities for a wide variety of industries.

Fast drying adhesive for many plastic films. Resists aromatic and aliphatic fuels, water, oil.

The solids weight is approximately 24%. The flash point is 35°F/3°C. The color is amber, the consistency is thin liquid, and the application method is spray or brush. The bond range holds up to 40 minutes. Peel strength is 27 PIW at 75°F (24°C); canvas to cold rolled steel at 2 inches/minute separation rate.

Information provided by 3M Adhesives Division.

Key Words: 3M Adhesives Division
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 1.37 MPa
@Temperature 24.0 °C
ASTM D1002-64
 59.0 psi
@Temperature 82.0 °C
Aluminum to aluminum at 0.1 inches/minute.  Bonds heat cured for 15 minutes at 325°F, 150 PSI.
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMMB06 / 53453

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.