MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Park Aerospace Nelco® N4000-11 BC® Buried Capacitance™ Epoxy Laminate and Prepreg
Categories: Polymer; Thermoset; Epoxy

Material Notes: The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved thermal, mechanical, and electrical performance in lead-free assembly and high layer count, sophisticated PWB designs. The Nelco N4000-11 BC® is offered as a buried capacitance solution, offering a greater degree of design freedom for smaller, more reliable assemblies.

Key Features and Benefits:

  • Tg >175ºC, thermal stability and moisture resistance
  • CAF Resistant
  • Low Z-axis expansion
  • Dicyandiamide (DICY) free, proprietary resin chemistry
  • Superior electrical properties
  • Buried Capacitance Solution
  • Optimized FR-4 processing

Applications/Qualifications:

  • High Density Interconnects
  • Lead-Free Assembly Substrate
  • Large Format Backplanes
  • Tight Tolerance Via to Via Applications
  • High I / O Count BGA Substrates
  • Extreme Layer count Multilayers
  • Lead-Free DCA Applications
  • High Temperature Underhood Automotive
  • Telecommunications Infrastructure
  • Sophisticated Data Storage Applications
  • RoHS Compliant
  • Meets IPC-4101/28, /83, /98, /99 Specifications

Information provided by Park Electrochemical Corp.

Key Words: EP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.96 g/cc0.0708 lb/in³50% Resin Content; Internal Method
Water Absorption 0.15 %0.15 %IPC-TM-650.2.6.2.1
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 1.23 kN/m7.00 pliat elevated temperature; IPC-TM-650.2.4.8.2a
 1.58 kN/m9.00 pliafter exposure to process solutions; IPC-TM-650.2.4.8
 1.58 kN/m9.00 pliafter solder float; IPC-TM-650.2.4.8
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.5
@Frequency 1e+9 Hz
3.5
@Frequency 1e+9 Hz
RF Impedance; IPC-TM-650.2.5.5.9
 3.5
@Frequency 2.50e+9 Hz
3.5
@Frequency 2.50e+9 Hz
Stripline; IPC-TM-650.2.5.5.5
 3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
TFC/LCR Meter; IPC-TM-650.2.5.5.3
Dielectric Strength 51.2 kV/mm1300 kV/inIPC-TM-650.2.5.6.2
Dissipation Factor  0.015
@Frequency 2.50e+9 Hz
0.015
@Frequency 2.50e+9 Hz
Stripline; IPC-TM-650.2.5.5.5
 0.018
@Frequency 1e+6 Hz
0.018
@Frequency 1e+6 Hz
TFC/LCR Meter; IPC-TM-650.2.5.5.3
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.21 - 1.38 J/g-°C0.290 - 0.330 BTU/lb-°FASTM E1461-92
Thermal Conductivity 0.401 - 0.599 W/m-K2.78 - 4.16 BTU-in/hr-ft²-°FASTM E1461-92
Glass Transition Temp, Tg 170 °C338 °FTMA; IPC-TM-650.2.4.24c
 >= 175 °C>= 347 °FDSC; IPC-TM-650.2.4.25c
Decomposition Temperature 345 °C653 °F5% weight loss; TGA; IPC-TM-650.2.4.24.6
Flammability, UL94 V-0V-0
 
Descriptive Properties
Methylene Chloride Resistance (% Weight Change)0.8IPC-TM-650.2.3.4.3
T260 (minutes)30IPC-TM-650.2.4.24.1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® H61 Thermally Conductive Epoxy
Park Aerospace Nelco® N4000-13 High-Speed Multifunctional Epoxy Laminate and Prepreg
Permabond ET536 Epoxy Resin
Raschig Group MELOPLAS® 181.5 MF
Epoxy Technology EPO-TEK® H61LV Thermally Conductive, Electrically Insulating Epoxy

PPARK116 / 89388

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.