Premi-Glas® 2203-25 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications. Key features and benefits are: - Enhanced product for higher UL long term operating temperature
- Good dimensional stability, including excellent thermal resistance
- Pigmentable for molded-in color; best appearance with mold texture
- Recognized by Underwriter's Laboratories, File #E42524
- Designed for compression molding in matched metal die molds.
A. Schulman has acquired this former Premix product line. |